MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Makrolon® SK1 sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Skylight prismatic Makrolon® SK1 sheet‘s prismatic pattern is optimized to diffuse and distribute light while maintaining high light transmission, making it the material of choice for daylighting applications. The product is available with a UV enhanced cap layer in both clear and white. Makrolon SK1 can be drape or thermoformed for use in contoured applications such as domed skylights. In either flat or contoured geometries, it has a higher impact resistance compared to acrylic or glass. Makrolon SK1 has a Limited Product Warranty against breakage, yellowing, and loss of light transmission.

Applications: Awnings, entryway canopies, skylights, barrel vaults, glazed archways, covered pedestrian walkways, and sloped, vertical, and curved glazing

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Tensile Strength, Yield 62.1 MPa9010 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 2.38 GPa345 ksiASTM D790
Compressive Strength 86.2 MPa12500 psiASTM D695
Compressive Modulus 2.38 GPa345 ksiASTM D695
Poissons Ratio 0.380.38ASTM E132
Shear Modulus 0.786 GPa114 ksiASTM D732
Shear Strength 41.4 MPa6000 psiYield; ASTM D732
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 32.0 J/cm
@Thickness 3.17 mm
60.0 ft-lb/in
@Thickness 0.125 in
no failure; ASTM D256
Impact Test >= 63.7 J
@Thickness 3.17 mm
>= 47.0 ft-lb
@Thickness 0.125 in
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C37.5 µin/in-°FASTM D696
Thermal Conductivity 0.195 W/m-K1.35 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Brittleness Temperature 93.3 °C200 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Transmission, Visible  72 %
@Thickness 3.00 mm
72 %
@Thickness 0.118 in
B72 White; ASTM D1003
 92 %
@Thickness 3.00 mm
92 %
@Thickness 0.118 in
Clear; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation
Thermal Ceramics Kaowool Bulk Fiber
Overview of materials for Polycarbonate, 20% Glass Filled
Morgan Advanced Ceramics Alphawool® Bulk Thermal Ceramic
Covestro Makrolon® Lumen XT sheet Polycarbonate

PCOVEST0855 / 202638

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.