MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow SYL-OFF® 297 ANCHORAGE ADDITIVE
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Adhesive

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.115 g/cc
@Temperature 25.0 °C
1.115 g/cc
@Temperature 77.0 °F
Kinematic Viscosity 4.0 cSt
@Temperature 25.0 °C
4.0 cSt
@Temperature 77.0 °F
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 51.0 °C124 °Fclosed cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4248
@Temperature 25.0 °C
1.4248
@Temperature 77.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Active Content (%)100
Appearanceliquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SYL-OFF® 7395 COATING
Dow SYL-OFF® SL 9151 RELEASE MODIFIER
Dow SYL-OFF® SL 9250 ANCHORAGE ADDITIVE
Overview of materials for Methacrylate Adhesive
Overview of materials for Polylactic Acid (PLA) Biopolymer

PDOWCO010 / 105711

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.