MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Baytec® MP-120 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec MP-120 is a diphenylmethane diisocyanate (MDI)-terminated polyether prepolymer based on polypropylene ether glycol (PPG).

Properties / Applications: Baytec MP-120 is a diphenylmethane diisocyanate (MDI)-terminated polyether prepolymer based on polypropylene ether glycol (PPG). It forms clear, moisture-cured films and is used in the formulation of one-component moisture-cured binders and two-component sealants and cast elastomers. Typical applications include rubber crumb binders, flexible caulks, and sealants. As with any product, use of Baytec MP-120 prepolymer in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 1.05 g/cc
@Temperature 80.0 °C
1.05 g/cc
@Temperature 176 °F
 1.09 g/cc
@Temperature 30.0 °C
1.09 g/cc
@Temperature 86.0 °F
Viscosity 2000 cP2000 cP
 100 cP
@Temperature 90.0 °C
100 cP
@Temperature 194 °F
 200 cP
@Temperature 70.0 °C
200 cP
@Temperature 158 °F
 400 cP
@Temperature 50.0 °C
400 cP
@Temperature 122 °F
 700 cP
@Temperature 40.0 °C
700 cP
@Temperature 104 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 279 MPa40500 psiASTM D412
Tensile Stress at Strain  12.5 MPa
@Strain 100 %
1810 psi
@Strain 100 %
ASTM D412
 19.0 MPa
@Strain 300 %
2760 psi
@Strain 300 %
ASTM D412
Elongation at Break 424 %424 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FPMCC
 
Descriptive Properties
AppearanceYellow liquid
Content11.7-12.3%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0250 / 202033

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.