ATOFINA Polypropylene PPH 9059 is homopolymer. Application ATOFINA Polypropylene PPH 9059 is intended for extrusion of bulk continuous filament (BCF) and continuous filament (CF) fibers. PPH 9059 has a special anti gas-fading formulation to significantly reduce yellowing in fibers. Information provided provided by Total Petrochemicals. Total Petrochemicals acquired former Fina and Atofina plastics product lines. |