MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AFE Technologies Cronite 657 Nickel Alloy Castings
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.

Information provided by AFE Technologies/North American Cronite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 450 MPa65300 psiAs Cast
Tensile Strength, Yield 230 MPa33400 psiAs Cast
Elongation at Break 10 %10 %As Cast; 5.65 A0.5
Rupture Strength  8.80 MPa
@Temperature 1000 °C,
Time 3.60e+7 sec
1280 psi
@Temperature 1830 °F,
Time 10000 hour
Stress Rupture
 15.0 MPa
@Temperature 950 °C,
Time 3.60e+7 sec
2180 psi
@Temperature 1740 °F,
Time 10000 hour
Stress Rupture
 23.0 MPa
@Temperature 900 °C,
Time 3.60e+7 sec
3340 psi
@Temperature 1650 °F,
Time 10000 hour
Stress Rupture
 34.0 MPa
@Temperature 850 °C,
Time 3.60e+7 sec
4930 psi
@Temperature 1560 °F,
Time 10000 hour
Stress Rupture
 48.0 MPa
@Temperature 800 °C,
Time 3.60e+7 sec
6960 psi
@Temperature 1470 °F,
Time 10000 hour
Stress Rupture
 64.0 MPa
@Temperature 750 °C,
Time 3.60e+7 sec
9280 psi
@Temperature 1380 °F,
Time 10000 hour
Stress Rupture
 100 MPa
@Temperature 700 °C,
Time 3.60e+7 sec
14500 psi
@Temperature 1290 °F,
Time 10000 hour
Stress Rupture

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes HR-224® Nickel Alloy
Haynes Hastelloy® X alloy, sheet

NCRON06 / 15991

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.