MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMW® D50F Silver Nickel Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: This material has been rebranded as NAECOMET® D50F.

CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices where auxiliary contacts are used. This type of material has good resistance to mechanical wear under high contact forces, and maintains a stable surface resistance.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.33625 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 40annealed
 89cold worked
Tensile Strength, Ultimate 27000 psiannealed
 50000 psicold worked
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000220 ohm-cm80 % IACS
 
Component Elements PropertiesOriginal ValueComments
Nickel, Ni 15 %
Silver, Ag 85 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® ELKONIUM 18 silver, copper, cadmium alloy
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Overview of materials for Silver Alloy
CMW® D50 Silver Nickel Contact Material ASTM B693
CMW® D505F Silver Nickel Contact Material

NCMW077 / 15890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.