MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for PVC, Flexible Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.920 - 1.89 g/ccAverage value: 1.29 g/cc Grade Count:1438
Viscosity 473000 - 473000 cP
@Temperature 177 - 177 °C
Average value: 473000 cP Grade Count:1
 473000 - 473000 cP
@Frequency 1000 - 1000 Hz
Average value: 473000 cP Grade Count:1
Viscosity Test 88.0 - 105 cm³/gAverage value: 99.3 cm³/g Grade Count:3
Linear Mold Shrinkage 0.00280 - 0.0310 cm/cmAverage value: 0.0140 cm/cm Grade Count:49
Melt Flow 0.420 - 460 g/10 minAverage value: 62.6 g/10 min Grade Count:11
Ash 0.0500 %Average value: 0.0500 % Grade Count:3
ASTM Color -2.21 - 96.7Average value: 33.5 Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35.0 - 110Average value: 74.7 Grade Count:1193
Hardness, Shore D 34.0 - 83.0Average value: 64.9 Grade Count:107
Hardness, Shore C 60.0 - 92.0Average value: 75.9 Grade Count:111
Tensile Strength, Ultimate 0.758 - 156 MPaAverage value: 17.0 MPa Grade Count:990
Tensile Strength, Yield 0.121 - 50.0 MPaAverage value: 14.1 MPa Grade Count:441
Elongation at Break 16.0 - 700 %Average value: 328 % Grade Count:1410
Modulus of Elasticity 0.00552 - 3.23 GPaAverage value: 2.40 GPa Grade Count:43
Flexural Modulus 0.0752 - 3.00 GPaAverage value: 2.38 GPa Grade Count:40
Izod Impact, Notched 0.267 - 12.3 J/cmAverage value: 4.45 J/cm Grade Count:47
Tear Strength 8.00 - 114 kN/mAverage value: 53.7 kN/m Grade Count:94
Dart Drop Total Energy 35.8 - 1110 J/cmAverage value: 145 J/cm Grade Count:17
Compression Set 13.0 - 80.0 %Average value: 34.0 % Grade Count:36
Clash Berg Modulus 0.00689 - 0.996 GPaAverage value: 0.341 GPa Grade Count:20
 0.00745 - 0.558 GPa
@Temperature -58.0 - -13.0 °C
Average value: 0.308 GPa Grade Count:24
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.50 - 5.60e+15 ohm-cmAverage value: 2.42e+14 ohm-cm Grade Count:90
 5.00 - 1.70e+14 ohm-cm
@Temperature 50.0 - 50.0 °C
Average value: 2.53e+13 ohm-cm Grade Count:17
Dielectric Constant 2.87 - 7.04Average value: 4.13 Grade Count:55
Dielectric Strength 11.8 - 98.0 kV/mmAverage value: 51.4 kV/mm Grade Count:6
Dissipation Factor 0.0280 - 0.190Average value: 0.0734 Grade Count:51
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:23
Hot Wire Ignition, HWI 15.0 - 120 secAverage value: 67.4 sec Grade Count:23
High Amp Arc Ignition, HAI 30.0 - 120 arcsAverage value: 87.3 arcs Grade Count:21
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 40.6 - 194 °CAverage value: 111 °C Grade Count:335
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 72.8 °CAverage value: 65.5 °C Grade Count:25
Vicat Softening Point 48.9 - 93.9 °CAverage value: 75.1 °C Grade Count:9
Minimum Service Temperature, Air -40.0 - -12.0 °CAverage value: -26.4 °C Grade Count:16
Brittleness Temperature -68.0 - 7.00 °CAverage value: -32.0 °C Grade Count:693
UL RTI, Electrical 50.0 - 90.0 °CAverage value: 79.0 °C Grade Count:30
UL RTI, Mechanical with Impact 50.0 - 90.0 °CAverage value: 54.4 °C Grade Count:15
UL RTI, Mechanical without Impact 50.0 - 90.0 °CAverage value: 77.2 °C Grade Count:28
Flammability, UL94 HB - 5VAGrade Count:42
Oxygen Index 21.0 - 51.0 %Average value: 28.3 % Grade Count:240
 
Optical PropertiesOriginal ValueComments
Haze 2.50 - 14.3 %Average value: 6.35 % Grade Count:8
Gloss 15.0 - 90.0 %Average value: 45.0 % Grade Count:4
Transmission, Visible 80.0 - 90.0 %Average value: 85.1 % Grade Count:17
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 190 °CAverage value: 169 °C Grade Count:39
Nozzle Temperature 160 - 190 °CAverage value: 178 °C Grade Count:38
Melt Temperature 110 - 210 °CAverage value: 179 °C Grade Count:340
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 56.0 %Average value: 56.0 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Molded
Overview of materials for PVC, Extruded
Overview of materials for PVC, Wire and Cable Grade
Overview of materials for PVC, Sheet Grade
Overview of materials for PVC, Transparent

O5642 / 78521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.