MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the user can change the properties of the product simply by changing the same combination of part-A and part-B liquid components. The material does not contain plasticizer so that it will not leach plasticizer to affect the other plastic material surrounding the gel part, or to cause a severe hardness change in long term use.

Possible application for this material includes potting and encapsulation of optical cables, manufacturing of puncture-free tire layer, cushioning and padding parts by open-cast molding, and many other custom applications. This material is not designed to be cast directly into flexible film casings.

Information provided by Northstar Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °FPrepolymer Temperature
 70.0 - 90.0 °FCuring Agent Temperature
Mold Temperature 70.0 - 90.0 °F
Cure Time 1.00 - 3.00 hour
@Temperature 25.0 °C
De-mold Time
 72.0 - 96.0 hour
@Temperature 25.0 °C
Complete Cure Cycle
Pot Life 11.0 - 12.0 min
 
Descriptive Properties
Curing AgentPAA-109
PrepolymerMPC-022
Weight Ratio1:10.391Prepolymer to Curing Agent Ratio, Shore Hardness OO <0.1
 1:7.422Prepolymer to Curing Agent Ratio, Shore Hardness OO 48-53
 1:7.917Prepolymer to Curing Agent Ratio, Shore Hardness OO 35-40
 1:8.412Prepolymer to Curing Agent Ratio, Shore Hardness OO 28-33
 1:9.402Prepolymer to Curing Agent Ratio, Shore Hardness OO 3-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)
3M Scotchkote™ 60EG 533 Urethane Elastomer
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast
Northstar Polymers MPC-W44A Polyurethane Gel
Resinlab® UR3005 Clear Two Part Urethane Elastomer

PNORTH870 / 162586

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.