MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Unival™ DMDF-6230 NT HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: Unival™ DMDF-6230 NT HDPE is specifically designed for use in either intermittent or continuous blow molding equipment to produce containers up to 20 gallons in size-applications that require the combination of outstanding environmental stress crack resistance (ESCR) and, high impact strength. Unival™ DMDF -6230 NT HDPE resin is also considered a multipurpose blow molding resin designed for the high speed production of blow molded containers used for packaging household industrial chemicals (e.g. detergents, bleach, fabric softeners), toiletries and cosmetics (e.g. shampoos, creams, lotions, etc.), health and medicinal aids. In addition, it can be blow molded into other thin walled parts and houseware items, and also can be extruded into profiles or sheets.
Main Characteristics:
  • Outstanding environmental stress crack resistance
  • High impact strength
  • Good extrusion characteristics
  • Formulated with a non-food grade antistatic agent
Compiles with: US FDA 21 CFR 175.105

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 175.105; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D792
ESCR 100% Igepal® 180 hour
@Temperature 50.0 °C
180 hour
@Temperature 122 °F
F50; ASTM D1693
Melt Flow  0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
25 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ASTM D2240
Tensile Strength at Break 31.0 MPa4500 psiASTM D638
Tensile Strength, Yield 23.4 MPa3400 psiASTM D638
Elongation at Break 900 %900 %ASTM D638
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Modulus 0.910 GPa132 ksi2% Secant; ASTM D790B
Tensile Impact Strength 210 kJ/m²100 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F
Crystallization Temperature 118 °C244 °F
Deflection Temperature at 0.46 MPa (66 psi) 62.2 °C144 °FUnannealed; ASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF576 / 311269

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.