MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo MAGNUM™ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resins are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming processes. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 2.4 to 11 ft-lb/in and heat distortion temperatures from 117 to 194°F are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars, and exterior trim parts requiring painting and plating. MAGNUM 347 HP ABS resin is a higher flow version of 342 EZ having slightly lower impact strength. The melt flow rate of approximately 12 g/10 min is often suitable for parts with long flow lines and minimal impact requirements.

Information provided by Styron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Maximum Moisture Content 0.100.10
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
12 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 41.4 MPa6000 psiType I, 51 mm/min; ASTM D638
Elongation at Break 30 %30 %Type I, 51 mm/min; ASTM D638
Elongation at Yield 2.5 %2.5 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.07 GPa300 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 65.5 MPa9500 psiType I, 1.3 mm/min; ASTM D790
Flexural Modulus 2.17 GPa315 ksiType I, 1.3 mm/min; ASTM D790
Izod Impact, Notched 1.30 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.44 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Dart Drop, Total Energy  73.9 J
@Thickness 3.20 mm,
Temperature 23.0 °C
54.5 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Total Energy; ASTM D3763
 85.0 J
@Thickness 3.20 mm,
Temperature 23.0 °C
62.7 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Peak Energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
@Thickness 3.20 mm
185 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
@Thickness 3.20 mm
165 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Vicat Softening Point 102 °C216 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 232 °C421 - 450 °F
Mold Temperature 26.7 - 48.9 °C80.1 - 120 °F
Drying Temperature 82.2 - 85.0 °C180 - 185 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Back Pressure 0.345 - 3.45 MPa50.0 - 500 psi
 
Descriptive Properties
Clamp Tonnage2.8-4.1 kN/cm2
Screw Compression Ratio1.5:1 to 3.5:1
Screw L/D Ratio0.834027777777778

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Trinseo MAGNUM™ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
INEOS Styrolution Terluran® GP-22 ABS
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled

PZZDWST068 / 142277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.