MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1199 X 115085 E Polyethylene Terephthalate Glycol Modified (PETG), Carbon Nanotube - ESD Protection
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.17 mm
0.0020 - 0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.6 MPa7200 psiASTM D 638
Elongation at Break 5.0 %5.0 %ASTM D 638
Tensile Modulus 2.69 GPa390 ksiASTM D 638
Flexural Strength 88.9 MPa12900 psiASTM D 790
Flexural Modulus 2.76 GPa400 ksiASTM D 790
Izod Impact, Unnotched 3.74 J/cm
@Thickness 3.17 mm
7.00 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 - 1000 ohm-cm10 - 1000 ohm-cmASTM D 257
Surface Resistance 1000 ohm - 1e+051000 ohm - 1e+05ESD STM11.11
Surface Resistivity per Square 10000 - 1.00e+6 ohm10000 - 1.00e+6 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Die Temperature 249 - 293 °C480 - 560 °F
Melt Temperature 249 - 293 °C480 - 560 °F
Drying Temperature 65.6 °C150 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -33.9 °C-29.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
RTP Company RTP 1199 A X 136859 B EG Polyethylene Terephthalate Glycol Modified (PETG); Permanently Static Dissipative - Extrusion Grade - ESD Protection
SunChemical Gwent C2011009D1 Curable Silver Range
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin
Eastman Tritan™ EX401 Copolyester

PQZWA10031 / 90463

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.