MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX974 Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 974 resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less electrostatic painting. NORYL GTX974 resin exhibits high impact resistance and is an excellent candidate for automotive painted applications such as body panels and fenders.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption 0.0700 %0.0700 %Injection Molding
 1.20 %1.20 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 4.2 %4.2 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 280 °C
12 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm
@Thickness 3.20 mm
0.013 - 0.016 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm
@Thickness 3.20 mm
0.011 - 0.014 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 280 °C
10 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527
 50.0 MPa7250 psi50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527
 55.0 MPa7980 psi50 mm/min; ASTM D638
Elongation at Break 30 %30 %50 mm/min; ISO 527
 50 %50 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.00 GPa290 ksi1 mm/min; ISO 527
 2.05 GPa297 ksi50 mm/min; ASTM D638
Flexural Strength 75.0 MPa10900 psiyield, 2 mm/min; ISO 178
 80.0 MPa11600 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.90 GPa276 ksi2 mm/min; ISO 178
 2.05 GPa297 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 180 J133 ft-lbASTM D256
 120 J
@Temperature -30.0 °C
88.5 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 J36.9 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 10000 ohm-cm1000 - 10000 ohm-cmSABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 180 °C
@Thickness 3.20 mm
356 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 175 °C347 °FRate B/50; ISO 306
 180 °C356 °FRate B/50; ASTM D1525
 180 °C356 °FRate B/120; ISO 306
 230 °C446 °FRate A/50; ISO 306
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 310 °C536 - 590 °F
Zone 2 280 - 300 °C536 - 572 °F
Zone 3 290 - 320 °C554 - 608 °F
Melt Temperature 290 - 320 °C554 - 608 °FInjection Molding
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82192 / 290139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.