EPOLENE® C-24 polymer is a branched low density polyethylene with a relatively high melt point and viscosity compared to other EPOLENE® C-type polymers. It is useful for extrusion coating of automotive carpet backing. It can also be used in compounding or injection molding applications. EPOLENE® C-24 polymer has good high temperature stability, low color, and low temperature flexibility. All tests are run at 23°C and 50% relative humidity. Information provided by Westlake Chemical. |