MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automotive and industrial coatings. The unique, disc-like or lamellar shape of Novacite® makes it useful for coating systems where low oil absorption and improved barrier properties are desired. In coatings, the lamellar plate overlap parallel to the substrate surface. It has a polar, wettable surface and is very transparent in the UV and visible range. Its structure alpha (low) quartz, which is stable to 573°C. The crystallography of Novacite shows it is an uncommon variety of quartz, with anhedral or subhedral crystals that cleave along the principal axis of the molecular structure.

Information provided by Malvern Minerals Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 77.2 MPa11200 psi
Tensile Strength, Yield 65.2 MPa
@Strain 0.2 %
9460 psi
@Strain 0.2 %
Elongation at Break 1.69 %1.69 %
Elongation at Yield 0.0 %0.0 %
Modulus of Elasticity 6.74 GPa978 ksi
Flexural Strength 77.2 MPa
@Strain 1.23 %
11200 psi
@Strain 1.23 %
Flexural Modulus 7.17 GPa1040 ksi
Compressive Yield Strength  140 MPa
@Strain 4.94 %
20300 psi
@Strain 4.94 %
 183 MPa
@Strain 28.3 %
26500 psi
@Strain 28.3 %
Compressive Modulus 6.34 GPa919 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  38.0 µm/m-°C
@Temperature -53.9 - 22.2 °C
21.1 µin/in-°F
@Temperature -65.0 - 72.0 °F
 38.0 µm/m-°C
@Temperature 22.2 - 73.9 °C
21.1 µin/in-°F
@Temperature 72.0 - 165 °F
 38.0 µm/m-°C
@Temperature -53.9 - 73.9 °C
21.1 µin/in-°F
@Temperature -65.0 - 165 °F
Thermal Conductivity 0.375 W/m-K2.60 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced
Overview of materials for Silicone Rubber
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for Epoxy, Molded, Glass Fiber Filler

PMALV950 / 149092

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.