MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NEXA® PFX9014 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consider. Applications include Aerospace, Automotive, Chemical, Food, Industrial, Pharmaceutical, Semiconductor, Nuclear, and Oil & Gas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 75
@Thickness 6.00 mm
65 - 75
@Thickness 0.236 in
DIN 53505
Tensile Strength >= 15.0 MPa>= 2180 psiDIN 53504
Elongation at Break >= 200 %>= 200 %DIN 53504
100% Modulus >= 4.00 MPa
@Strain 100 %
>= 580 psi
@Strain 100 %
DIN 53504
Compression Set  <= 18 %
@Temperature 200 °C,
Time 259000 sec
<= 18 %
@Temperature 392 °F,
Time 72.0 hour
DIN 53517
 <= 22 %
@Temperature 260 °C,
Time 259000 sec
<= 22 %
@Temperature 500 °F,
Time 72.0 hour
DIN 53517
 <= 22 %
@Temperature 200 °C,
Time 605000 sec
<= 22 %
@Temperature 392 °F,
Time 168 hour
DIN 53517
 <= 27 %
@Temperature 290 °C,
Time 259000 sec
<= 27 %
@Temperature 554 °F,
Time 72.0 hour
DIN 53517
 <= 31 %
@Temperature 316 °C,
Time 259000 sec
<= 31 %
@Temperature 601 °F,
Time 72.0 hour
DIN 53517
 <= 33 %
@Temperature 275 °C,
Time 605000 sec
<= 33 %
@Temperature 527 °F,
Time 168 hour
DIN 53517
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 334 °C633 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound
Geon® Performance Solutions Vinyl Flexible XV3796 Polyvinyl Chloride, Flexible
Precision Polymer Engineering S60A Silicone Rubber
Precision Polymer Engineering V70Q Fluoroelastomer Compound
Colorite Polymers Self Frosting™ 6511SF Vinyl Compound

PNEXA909 / 123943

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.