MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 0201FX Plastomer for Blown Film Applications  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology. Designed for use in both monolayer and multilayer industrial blown film applications requiring outstanding sealability and toughness. The are formulated with slip and antiblock for packaging and lamination applications.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccExxonMobil Method
Thickness 1.25 mil
Melt Flow 1.1 g/10 minExxonMobil Method
Antiblock Level 3000 ppm
Slip Level 1200 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 720 psi2% Offset; ASTM D882
Film Tensile Strength at Yield, TD 630 psi2% Offset; ASTM D882
Film Elongation at Break, MD 470 %ASTM D882
Film Elongation at Break, TD 720 %ASTM D882
Film Elongation at Yield, MD 9.5 %ASTM D882
Film Elongation at Yield, TD 7.8 %ASTM D882
Puncture Energy 22.1 in-lbExxonMobil Method
Elmendorf Tear Strength, MD 120 g/milASTM D1922
Elmendorf Tear Strength, TD 384 g/milASTM D1922
Dart Drop 568 g/milASTM D1709A
Film Tensile Strength at Break, MD 9260 psiASTM D882
Film Tensile Strength at Break, TD 8770 psiASTM D882
1% Secant Modulus, MD 9900 psiASTM D882
1% Secant Modulus, TD 10800 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 203 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 79.0 °CExxonMobil Method
Vicat Softening Point 181 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.4 %ASTM D1003
Gloss 78 %ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer and PPA

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 201 Plastomer for Blown Film Applications
ExxonMobil EXACT™ 0201HS Plastomer for Blown Film Applications
ExxonMobil EXACT™ 201 Plastomer for Polymer Modification
TIMCAL TIMREX® KS300-1250 Primary Synthetic Graphite
LyondellBasell Adsyl™ 5 C 37 F Polyolefin

PEXB339 / 37644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.