MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abhar Polymer Compounds APXLP13 /APCAT13N Silane Cross-linkable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: APXLP13 is a XLPE pre-grafted polyethylene which can be processed in combination with its catalyst master batch (APCAT13N) in conventional extruders. End product crosslinking occurs when the PABHAR is exposed to moisture.

Application: APXLP13 is suitable for insulation of low voltage wiring and power cables for the range up to 1kV. It’s suitable for use in high speed XLPE Cable insulation lines.

Specification: The catalyst masterbatch APCAT13N in combination with the base PABHAR APXLP13 meets the applicable requirements given below when processed using extrusion practice and testing procedure:

  • BS 7870-5
  • IEC 60502-1
Typical values reported above (except MFI) are obtained from samples cured in hot water (7 hours @ 95°C)

Information provided by Abhar Polymer Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 - 0.925 g/ccASTM D 792 / IEC 60811-1-3
Melt Flow 2.5 - 3.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature <= 35.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48 - 52
@Time 15.0 sec
ASTM D2240
Tensile Strength 11.25 - 15.0 MPaafter ageing 10 days at 150°C; IEC 60811-1-2
 >= 15.0 MPaIEC 60811-1-1
Elongation at Break 225 - 300 %after ageing 10 days at 150°C; IEC 60811-1-2
 >= 300 %IEC 60811-1-1
Tensile Set <= 10 %
@Pressure 0.200 MPa,
Temperature 200 °C
Permanent elongation after cooling; IEC 60811-2-1
 <= 100 %
@Pressure 0.200 MPa,
Temperature 200 °C
Elongation under load; IEC 60811-2-1
 
Processing PropertiesOriginal ValueComments
Zone 1 160 - 180 °C
Zone 2 180 - 200 °C
Zone 3 190 - 210 °C
Zone 4 200 - 220 °C
Die Temperature 220 - 230 °C
Head Temperature 210 - 230 °C
Screw Cooling Temperature 70.0 - 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABHAR002 / 249435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.