MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® PLS95G50DH2 BK261 PA66/6T-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66

Material Notes: 50% Glass Reinforced, Heat Stabilized, Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccDAM; ISO 1183
Water Absorption 4.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 125 cm³/gsulfuric acid 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPa50% RH; ISO 527-1/-2
 240 MPaDAM; ISO 527-1/-2
Elongation at Break 2.6 %DAM; ISO 527-1/-2
 4.0 %50% RH; ISO 527-1/-2
Tensile Modulus 12000 MPa50% RH; ISO 527-1/-2
 17000 MPaDAM; ISO 527-1/-2
Flexural Strength 370 MPaDAM; ISO 178
Flexural Modulus 16000 MPaDAM; ISO 178
Poissons Ratio 0.3350% RH
 0.33DAM
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 16.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 10000 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 6500 MPa1000h; 50% RH; ISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°CDAM; ISO 11359-1/-2
 5.00 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 67.0 µm/m-°CDAM; ISO 11359-1/-2
 56.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 120 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Melting Point 267 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 263 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 254 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 65.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 42.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 °COptimum, Injection
 285 - 305 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66/6T,GF50,M1CGHR,S12-160
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66/6T-GF50<ISO 11469
PolymerPA66/6T-GF50
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66/6T-GF50ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5487a / 291032

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.