MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NuSil MED-4128 Silicone, One Part High Consistent Elastomer - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: HCRs can be used for extrusion of tubing and profiles (rod or ribbon), in calendared sheeting for die-cutting, or in compression or transfer molded parts such as balloons, gaskets or o-rings. HCRs are clay-like in the uncured state and when cured generally exhibit very high mechanical properties and low modulus.

Important Properties: HCRs with a peroxide cure system have a long history in implant applications. The cure mechanism can be vinyl specific or non vinyl specific. Non vinyl specific peroxide catalysts are more commonly used with HCRs than vinyl specific peroxide catalysts. Features of peroxide cure high consistency rubbers include the following:

  • One or two part
  • Indefinite work time
  • Heat required
  • Acid or alcohol byproducts
  • Post cure required
  • % shrinkage ~2 -5%
Comments: Low Tension Set, Uncatalyzed

Cure System: Peroxide

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525Typical
 20 - 3020 - 30Certified
Tensile Strength at Break 5.50 MPa798 psiCertified
 7.40 MPa1070 psiTypical
Tensile Stress at Strain 0.621 MPa
@Strain 200 %
90.0 psi
@Strain 200 %
Elongation at Break 700 %700 %Certified
 825 %825 %Typical
Tear Strength 7.01 kN/m40.0 pliCertified
 13.1 kN/m75.0 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 116 °C
0.0833 hour
@Temperature 241 °F
 120 min
@Temperature 200 °C
2.00 hour
@Temperature 392 °F
Post
 
Descriptive Properties
Mix Ratio1 Part
Plasticity71 mils

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNUSIL419 / 142143

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.