MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mytex Polymers AS65K-2ATM Polypropylene, Talc filled, Compounded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology. This material exhibits high flow and good processability characteristics.

Key Applications: Non-painted instrument panel

Information provided by Mytex Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
Melt Flow 18 g/10 minASTM D1238
Ash 25 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6015 sec; ISO 868
Tensile Strength, Yield 20.0 MPa50 mm/min; ISO 527
Flexural Modulus 2170 MPaTangent; 1.3 mm/min; ISO 178
Izod Impact, Notched (ISO) 35.0 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CISO 75-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman TPP20AF01HB 20% Talc-Filled Homopolymer Polypropylene
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled
LyondellBasell Hifax HKC 426P BLACK Polypropylene with 20% Talc Filler
Mytex Polymers AS23KW-01 Polypropylene, Talc filled, Compounded
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded

PMYTEX020 / 90310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.