MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® LC7202 BK PA
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDAM; ISO 1183
Moisture Absorption 1.00 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 166 cm³/gDAM; ISO 307, 1157, 1628
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPa50% RH; ISO 527-1/-2
 30.0 MPaDAM; ISO 527-1/-2
Elongation at Break >= 200 %Nominal; 50% RH; ISO 527-1/-2
 >= 200 %Nominal; DAM; ISO 527-1/-2
Elongation at Yield 5.7 %DAM; ISO 527-1/-2
 7.5 %50% RH; ISO 527-1/-2
Tensile Modulus 900 MPa50% RH; ISO 527-1/-2
 1000 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.4550% RH
 0.45DAM
Charpy Impact Unnotched 160 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 160 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 175 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 230 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 23.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 25.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 100 kJ/m²
@Temperature 23.0 °C
Partial Break; DAM; ISO 179/1eA
 110 kJ/m²
@Temperature 23.0 °C
Partial Break; 50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 168 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 303 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 122 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
Melting Point 214 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 55.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C10°C/min; DAM; ISO 11357-1/-2
Flame Spread 17.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 - 240 °CRange, Extrusion
Drying Temperature 75.0 - 80.0 °CExtrusion
Dry Time 3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 
Descriptive Properties
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA612-I,,ECG1H,S10-010
PolymerPA*...
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5475a / 291029

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.