MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Silicone Polyurethane, Polycarbonate Based; Silicone, Thermoplastic

Material Notes: Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-Energy Silicone Surface; Outstanding Oxidative Stability; Hydrophobic; High Tensile Strength; Optically Clear.

PurSil™ silicone-polyetherurethane and CarboSil™ silicone-polycarbonateurethane are true thermoplastic copolymers containing silicone in the soft segment. These high-strength thermoplastic elastomers are prepared through a multi-step bulk synthesis where polydimethylsiloxane (PSX) is incorporated into the polymer soft segment with polytetramethyleneoxide (PTMO) (PurSil) or an aliphatic, hydroxyl-terminated polycarbonate (CarboSil). The hard segment consists of an aromatic diisocyanate, MDI, with a low molecular weight glycol chain extender. The copolymer chains are then terminated with silicone (or other) Surface-Modifying End Groups™. Aliphatic (AL) versions of these materials, with a hard segment synthesized from an aliphatic diisocyanate, are also available.

PurSil and CarboSil can be melt fabricated by conventional extrusion, injection molding, or compression molding techniques. Rod, pellet, and tubing extruded from these materials displays an excellent surface finish and low gel content. In addition, these materials are heat-sealable, readily blended with fillers, and easily post-formed.

Information provided by the manufacturer, Polymer Technology Group.

Key Words: The Polymer Technology Group; Polyurethane; TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.011 cm/cm4.0" disk; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
Tensile Strength, Ultimate 39.9 MPaASTM D1708
Tensile Stress at Strain 7.20 MPa
@Strain 50 %
ASTM D1708
Elongation at Break 420 %ASTM D1708
Flexural Yield Strength 2.00 MPa5% deflection; ASTM D-790
Flexural Modulus, 1% Secant 0.0414 GPaASTM D790
Tear Strength 540 pliDie "C"; ASTM D624
Taber Abrasion, mg/1000 Cycles 20H-18 wheel; ASTM D-1044
Compression Set 26 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.7
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.7 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
ASTM E831
Vicat Softening Point 84.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Manufacturer notes 'clear' but doesn't quantify
 
Processing PropertiesOriginal ValueComments
Processing Temperature 185 - 200 °CExtrusion
Drying Temperature 82.0 - 104 °C
Dry Time 4 - 6 hourto moisture < 0.01%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane
DSM Biomedical Calo-MER™ 35 Shape Memory Thermoplastic
DSM Biomedical Calo-MER™ 40 Shape Memory Thermoplastic
Indium Corp. Indalloy 128 Pure Tin
DSM Biomedical Calo-MER™ 45 Shape Memory Thermoplastic

PBIOC0 / 27165

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.