MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Asahi Kasei Stylac™ 26 ABS Polymer, High Stiffness
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes:

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 19 g/10 min
@Load 9.18 kg,
Temperature 220 °C
19 g/10 min
@Load 20.2 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ISO 2039-2
 113
@Thickness 2.50 mm
113
@Thickness 0.0984 in
Tensile Strength, Yield 58.0 MPa8410 psi50mm/min; ISO 527-1
Flexural Strength 92.0 MPa13300 psi2mm/min; ISO 178
Flexural Modulus 2.90 GPa421 ksi2mm/min; ISO 178
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FRelative Thermal Index; UL 746A
Hot Ball Pressure Test 90.0 °C194 °FRegistered Number: B-1558; EMAC
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75-1,2
Vicat Softening Point 103 °C
@Load 5.10 kg
217 °F
@Load 11.2 lb
ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced
Asahi Kasei Stylac™ 10 ABS Polymer, High Stiffness

PASAHI8258 / 221282

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.