MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dover Chemical DOVERMULSE H1020P Polyisobutylene succinic anhydride
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Dovermulse H1020-P is a polyisobutylene succinic anhydride prepared from 950 Mol Wt PIB and maleic anhydride. The PIBSA has been prepared via the thermal route, so there is no residual chlorine. Dovermulse H1020-P may be used as a dispersant or emulsifier in various applications. Dovermulse can be based on other molecular weights of either HR or conventional PIB.

Information provided by DoverChem

Key Words: CAS# 67762-77-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 100°C (212°F) 220 cSt220 cSt
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 4646[mgKOH/g]
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl <= 0.010 %<= 0.010 %residual
 
Descriptive Properties
AppearanceThick Amber liquid
Free Maleic Acid, %0.25
Hydrolysis, %<5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dover Chemical DOVERMULSE H1010P Polyisobutylene succinic anhydride
Dover Chemical DOVERMULSE H1000 Polyisobutylene succinic anhydride
Celanese 50000875 3-Methoxybutanol
Parker Chomerics CHO-BOND® 4660 Conductive Caulk/Sealant
ExxonMobil Escorez™ 5490 Tackifying Resin

WDOVER156 / 217775

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.