MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ PPE Powders + Concentrates 6850H
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: NORYL™ 6850H resin concentrate is an non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This material is in granule form and is optimized for blending with polystyrene resins. NORYL 6850H resin may be an excellent candidate in microwavable food packaging applications. This product is not certified per food contact regulations in US + EUR. Certification would be dependent on end-part testing.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Moisture Absorption 0.0600 %0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 140000 cP140000 cPmelt; ISO 11443
 20 cP
@Load 5.00 kg,
Temperature 280 °C
20 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 18.0 MPa2610 psi50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
Elongation at Break 51 %51 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.34 GPa339 ksi1 mm/min; ISO 527
Flexural Strength 97.0 MPa14100 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.38 GPa345 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 126 °C259 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 141 °C286 °FRate B/50; ISO 306
 147 °C297 °FRate B/120; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82240 / 290187

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.