MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® FR70M30V0 NC010 PA66-MD30FR(17)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: 30% Mineral Reinforced, Flame Retardant, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccDAM; ISO 1183
Melt Density 1.40 g/cc
@Temperature 290 °C
Water Absorption 4.0 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50% RH; ISO 527-1/-2
 73.0 MPaDAM; ISO 527-1/-2
Elongation at Break 2.0 %DAM; ISO 527-1/-2
 6.0 %50% RH; ISO 527-1/-2
Tensile Modulus 3500 MPa50% RH; ISO 527-1/-2
 6500 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.35DAM
 0.3750% RH
Izod Impact, Notched (ISO) 1.90 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 2.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 2.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 2.50 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 19.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 20.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 20.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 30.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 2.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 2.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 3.00 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance >= 1.00e+15 ohm50% RH; IEC 62631-3-2
Dielectric Constant 3.7
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.1
@Frequency 100 Hz
DAM; IEC 62631-2-1
 4.2
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 9.1
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 33.0 kV/mm50% RH; IEC 60243-1
 40.0 kV/mmDAM; IEC 60243-1
Dissipation Factor 0.014
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.014
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.041
@Frequency 100 Hz
50% RH; IEC 62631-2-1
 0.050
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 325 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 64.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 81.0 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 1.70 J/g-°C
@Temperature 290 °C
Melt
Thermal Conductivity 0.230 W/m-K
@Temperature 290 °C
Melt
Melting Point 263 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 238 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 145 °CDAM; ISO 75-1/-2
Vicat Softening Point 235 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 80.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 V-2
@Thickness 0.750 mm
DAM; IEC 60695-11-10
 V-0
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 5VA
@Thickness 1.50 mm
DAM; IEC 60695-11-20
Glow Wire Ignition Temperature 800 °C
@Thickness 0.750 mm
DAM; IEC 60695-2-13
 800 °C
@Thickness 1.00 mm
DAM; IEC 60695-2-13
 800 °C
@Thickness 1.50 mm
DAM; IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
DAM; IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesFlame retardant
 Release agent
Drying RecommendedyesInjection
FMVSS ClassDNIISO 3795 (FMVSS 302)
ISO designationISO 16396-PA66,MD30 FR(17),M1F1GNR,S14-060
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66-MD30FR(17)<ISO 11469
PolymerPA66-MD30 FR(17)
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66-MD30FR(17)ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® FR50 BK505 PA66-GF25FR(17)
Celanese Celanex® 3316 PBT, 30% Glass Reinforced
DuPont Mobility and Materials Zytel® FR70G25V0 NC010 PA66-GF25FR(17)
Celanese Zytel® FR50 NC010 PA66-GF25FR(17)
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35

PDSX5427 / 198067

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.