MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celstran® PPS-GF50-01 AD3002 Black PPS, 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: 50% long strand glass fiber reinforced polyphenylene sulfide

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/ccASTM D792
Density 1.72 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPa5mm/min; ISO 527-2/1A
 25600 psiASTM D638
 26100 psi
@Temperature -40.0 °C
ASTM D638
Elongation at Break 1.0 %ASTM D638
 1.0 %5mm/min; ISO 527-2/1A
 0.95 %
@Temperature 4.44 °C
ASTM D638
Tensile Modulus 19000 MPa50mm/min; ISO 527-2/1A
 2.93e+6 psiASTM D638
 3.11e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 280 MPaISO 178
 38400 psiASTM D790
 39100 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 18550 MPaISO 178
 2.51e+6 psiASTM D790
 2.71e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 6.90 ft-lb/inASTM D256
 7.00 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Charpy Impact, Notched 28.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 282 °CISO 75-1, -2
 540 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 160 °Ccavity
Feed Temperature 20.0 - 50.0 °C
Zone 1 285 - 295 °C
Zone 2 290 - 300 °C
Zone 3 295 - 305 °C
Zone 4 300 - 310 °C
Die Temperature 290 - 300 °C
Melt Temperature 300 - 310 °C
Drying Temperature 130 - 140 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry)
DuPont Mobility and Materials Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

PHCQ251 / 178706

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.