LNP LUBRICOMP RX05050 compound is based on Nylon 6/6 resin containing 10% PTFE, 10% aramid fiber and 10% carbon fiber. Added features of this grade include: Electrically Conductive, Wear Resistant. Features: Wear resistant,Electrically Conductive Information provided by SABIC |