MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANTHANE® 125K-AS-Compound TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: DANTHANE_ 125K-AS-Compound is a polyurethane elastomer based on polyester. This compound is fitted antistatic with carbon black. DANTHANE_ 125K-AS-Compound is processed by melt calender, flat film extrusion and injection molding. This special TPU is used for the production of coatings for films, textiles and divers injection molding parts.

Application: DANTHANE_ 125K-AS-Compound is a special TPU type for calendering and extrusion of electrical conductive or antistatic TPU-foils and TPU–films. The direct extrusion of coating films on textiles or other supporting materials is possible. Typical applications are the processing of membrane foils, decor foils, foils for hoses and cables. It can also be used for the coating of conveyor belts and driving belts.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN 53.479
Melt Flow 50 - 70 g/10 min
@Load 10.0 kg,
Temperature 220 °C
50 - 70 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585DIN 53.505
Tensile Strength 30.0 MPa4350 psiDIN 53.504
Elongation at Break 500 %500 %DIN 53.504
Tear Strength 110 kN/m628 pliDIN 53.515
Abrasion 2525[mm³]; DIN 53.516
 
Thermal PropertiesMetricEnglishComments
Melting Point 155 - 165 °C311 - 329 °FKofler
Softening Point 130 - 140 °C266 - 284 °FCharacteristic of the film
 130 - 145 °C266 - 293 °FKofler
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 190 °C356 - 374 °FCompression zone, Extruded
 190 - 200 °C374 - 392 °FMetering zone, Extruded
 200 °C392 °FCompression zone, Injection
 210 °C410 °FMetering zone, Injection
Feed Temperature 170 - 180 °C338 - 356 °FExtruded
 195 °C383 °FInjection
Die Temperature 195 - 200 °C383 - 392 °FExtruded
 210 °C410 °FInjection
Mold Temperature 32.0 °C89.6 °FInjection
Injection Pressure 8.00 - 11.0 MPa1160 - 1600 psi
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectBlack colored pearl granule(RAL 9005)
 black, elasticCharacteristic of the film
Electrical conductivity120.00 – 190.00 K?

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ138 / 294558

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.