Description: The primer is a complex solution of reactive silanes in a volatile solvent. Upon application, the carrier solvent evaporates leaving behind a layer amenable to bonding various silicone elastomers. An appropriate combination of primer and application procedure can yield a bonding layer capable of adhering silicone to a variety of substrates. Primers typically enable adhesion at relatively low temperature. Key Features - Particularly suited for addition-cure (Pt) silicone formulations
- Will not haze, crack, or craze polycarbonate or acrylic
- Designed to impart strong adhesion to substrates used in electronics manufacture
- One-component, carried in alcohols
Application: QSil Primer #8 is for use with condensation and addition cure silicone elastomers and is safe to use on polycarbonate and acrylic.Information provided by CHT Group |