MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Weartech International WT-4 Cobalt Hardfacing & Wear Resistant Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: Applications: battery mold, guide rolls for galvanizing tanks

Information provided by Weartech International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 44 - 50
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.80 %
Chromium, Cr 30 %
Cobalt, Co 47.7 - 53.7 %
Iron, Fe <= 3.0 %
Nickel, Ni <= 3.0 %
Silicon, Si 1.5 %
Tungsten, W 14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
414 Stainless Steel, tempered at 508°C
AISI Type S21900 (21-6-9) Stainless Steel, 30% final cold reduction
AISI Type 430F(Se) Stainless Steel annealed bar
405 Stainless Steel, annealed, plate
347 Stainless Steel, annealed, plate

NWEART003 / 142540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.