MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Bergamid™ B700 UF black Polyamide 6 (Nylon 6), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³±0.03 g/cm³; DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa
@Temperature 23.0 °C
7980 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 1.50 GPa
@Temperature 23.0 °C
218 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.630 J/cm²
@Temperature -30.0 °C
3.00 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.840 J/cm²
@Temperature 23.0 °C
4.00 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
Maximum Service Temperature, Air 85.0 °C185 °FContinuous (GTP 50% Tensile); IEC 60216
 160 °C320 °FShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
ALL; Internal Method
Glow Wire Ignition Temperature 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
 
Descriptive Properties
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
K-Value74.0 to 78.0No Standard; 96% H2SO4
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6)
Avient Bergamid™ B700 UF Polyamide 6 (Nylon 6)
Avient Bergamid™ B700 UF black Polyamide 6 (Nylon 6), DAM
Epsan Eplamid 6 GX0 30 NC Q1D0C001 Polyamide 6
Envalior Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber

PH0POL1470 / 146039

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.