MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Sustane™ CG 200 Fragrance fixative
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Sustane™ CG 200 fragrance fixative promotes longevity in fine fragrance and personal care formulations. Sustane is a specially formulated sucrose acetate isobutyrate (SAIB) derived from natural sugar in an easy-to handle liquid. Sustane interacts with specific molecules in fragrance mixtures to lower vapor pressure and slow down evaporation. When you formulate with Eastman Sustane fragrance fixative, you give your customers what they want: a fragrance that lasts all day.

Applications

  • Fragrance ingredients
Key Attributes
  • Active ingredient (SAIB) derived from natural sugar
  • Colorless
  • Cosmetic grade
  • Inherently biodegradable
  • Leaves no residue on skin
  • Odorless
  • Pours readily at room temperature
  • Provides longevity to a wide variety of fragrances
  • Safe and easy handling

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Viscosity 1000 cP1000 cP
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.200<= 0.200[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 28.0 °C82.4 °FSetaflash Closed Cup
 
Descriptive Properties
Color<200Pt-Co
Content9-11%Ethyl Alcohol
FormPourable Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4150 / 323773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.