MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ZEON Zeotherm® 131-90B Thermoplastic Vulcanizate, TPV/TPE  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Blow moldable and extrusion grade with exceptional high heat and oil resistance of 150°C continuous, 175°C intermittent use; Thermoplastic vulcanizate (TPV) made of dynamically vulcanized polyacrylate rubber and polyamide 6. Excellent 3D and suction blow

Information provided by Zeon Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868, 15s
Hardness, Shore D 28ISO 868, 15s
Tensile Strength 14.0 MPaASTM D412
Elongation at Break 240 %ASTM D412
100% Modulus 0.00980 GPa
@Strain 100 %
ASTM D412
Flexural Modulus 95.0 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
 175 °C
Brittleness Temperature -44.0 °CASTM 2137
 
Descriptive Properties
ColorBlack
FeaturesACM + PA6 (nylon 6)
Physical FormPellets
Primary Marketautomotive
Processing Methodblow molding; injection molding; extrusion
REACHYes
RoHSYes
Typical applicationsautomotive boot

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ZEON Zeotherm® 100-80B Thermoplastic Vulcanizate, TPV/TPE
ZEON Zeotherm® 110-70B Thermoplastic Vulcanizate, TPV/TPE
ZEON Zeotherm® 100-70B Thermoplastic Vulcanizate, TPV/TPE
ZEON Zeotherm® 151-40D Thermoplastic Vulcanizate, TPV/TPE
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer

PZEOND03 / 206362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.