MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wall Colmonoy COLMONOY® 56 PTA Nickel-Base Hard-Surfacing Alloy With Chromium Boride
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Nickel Alloy

Material Notes: Colmonoy 56 PTA is a premium alloy specially formulated for plasma transferred arc (PTA) application on new and worn extrusion screws. High levels of chromium and carbon produce large populations of chromium carbides for superior abrasion and corrosion resistance. The optimized PTA formulation also has reduced boron and increased silicon for better weldability and puddle control.

Applications: Colmonoy 56PTA is specifically formulated for overlaying the flights of new and rebuilt extrusion and injection molding screws. It also has applications in the food processing industry on feed screws, air locks and scraper blades. Colmonoy 56PTA is also available in other powder forms and as rod for application on extrusion screws, wear rings, shafts, sleeves cement gate valves, forming and drawing dies, and centrifugal pump parts.

Information provided by Wall Colmonoy Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.33 g/ccapparent
 8.01 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 46 - 51single pass
 53 - 58double pass
 
Thermal PropertiesOriginal ValueComments
Melting Point 1940 °F
 
Component Elements PropertiesOriginal ValueComments
Boron, B 1.9 %
Carbon, C 0.90 %
Chromium, Cr 18 %
Iron, Fe 5.4 %
Nickel, Ni 68.5 %As Balance
Silicon, Si 5.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 56 Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides
Wall Colmonoy COLMONOY® 57 PTA Nickel-Base Hard-Surfacing Alloy
Wall Colmonoy COLMONOY® 83 PTA Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
Wall Colmonoy COLMONOY® 88 Hard-Surfacing Alloy
Wall Colmonoy COLMONOY® 21A PTA Nickel Alloy with Tungsten Carbide

NWALL12 / 19779

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.