Type: Pearlstick® 5713 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU). Features: It has the highest heat resistance of any Pearlstick TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and bond strengths can be achieved with the addition of diisocyanates, peroxides, epoxies and polyfunctional amides. Uses: Hot melt adhesive, solution cast films for lamination on fabrics. Information provided by The 159 Corporation |