MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-OP902 Highly Effective Non-Halogenated Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEM-OP902, developed by GYC GROUP, is an organic phosphate nonhalogenated flame retardant that provides excellent flame retardant performance to the end-products owing to its high content of phosphorus. For its excellent physical properties, processability, hydrolysis-resistibility, and pigmentability, GOYENCHEM-OP902 is commonly used in thermoplastics and thermoset plastics especially for engineering plastics (PA6, PA66, PET, PBT…) that high processing temperature and thermal stability are required.

Intro: GO YEN CHEMICAL CO. LTD. is the largest manufacturer of flame retardants and fine chemicals in Taiwan. We provide a series of total solutions for our customers to satisfy their needs. GOYENCHEM-OP902, developed by GYC GROUP, is an organic phosphate nonhalogenated flame retardant that provides excellent flame retardant performance to the end-products owing to its high content of phosphorus. For its excellent physical properties, processability, hydrolysis-resistibility, and pigmentability, GOYENCHEM-OP902 is commonly used in thermoplastics and thermoset plastics especially for engineering plastics (PA6, PA66, PET, PBT…) that high processing temperature and thermal stability are required.

Advantages:

  • Non-halogenated & eco-friendly flame retardant
  • Provide excellent flame retardant performance to the end-products
  • Excellent physical properties, processability
  • Excellent electrical characteristic
  • Great pigmentability
  • Non-hygroscopic
  • High thermal stability which is applicable at engineering plastic processing
  • Exceptional hydrolysis-resistibility
  • Great compatibility
  • Improve production efficiency and quality
  • Will not cause blooming/migration
Applications:
  • Any thermoplastics and thermoset plastics
  • High-end engineering plastics: PA, PET, PBT
  • PA6, PA66, PA6 glass fiber, PA66 glass fiber
  • Modified polyester: PCT?PCTA?PETG?PCTG

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.700 g/cc
Volatiles >= 0.30 %
Particle Size 20 - 40 µmD50
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature >= 375 °C
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 23.3 - 24 %
 
Descriptive Properties
AppearanceFine powder
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN007 / 266315

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.