BL4 (HM 8255) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, easily processable, high stiffness and impact good stress cracking resistance and even good molding surface finish. Applications: general purpose grade for containers from 1 to 500 L capacity. Information provided by Iran Petrochemical Commercial Co. |