MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 101 FR Polypropylene (PP) Glass Fiber - Flame Retardant - UL94 V-0  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D 792
Water Absorption 0.010 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D 570
Additive Loading 10 %Primary Additive
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
ASTM D 955
Melt Flow 2.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D 785
Tensile Strength at Break 5500 psiASTM D 638
Elongation at Break 2.0 - 3.0 %ASTM D 638
Tensile Modulus 750 ksiASTM D 638
Flexural Strength 9500 psiASTM D 790
Flexural Modulus 550 ksiASTM D 790
Izod Impact, Notched 0.700 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 3.50 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 490 V/milin oil; S/T; ASTM D 149
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 80 secASTM D 495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 300 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 280 °FASTM D 648
Vicat Softening Point 150 °C50 °C/h, 10 N; ASTM D 1525
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 - 450 °F
Mold Temperature 90.0 - 150 °F
Drying Temperature 175 °F
@Time 7200 sec
Injection Pressure 10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 104 CC FR A UV Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - Non- PBB/PBDE - UV Stabilized
RTP Company RTP 199 x 117565 A Polypropylene (PP), Flame Retardant - Low Flow - High Impact - Preliminary Datasheet
RTP Company RTP 103 FR Polypropylene (PP), Glass Fiber - Flame Retardant - UL94 V-0
RTP Company RTP 101 CC HI FR Polypropylene (PP) High Impact - Glass Fiber - Chemically Coupled - Flame Retardant - UL94
RTP Company RTP 101 CC FR Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - UL94 V-0

PQZVA1125 / 120459

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.