MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akrochem Ethanox® 330 Antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Ethanox 330 antioxidant is a highly effective, non coloring, odorless antioxidant for plastics, resins, elastomers and waxes. It has very low volatility and is outstanding in applications requiring high processing temperatures. It is safe and effective for use in a wide variety of polymers. If your polymer is sanctioned by the FDA for use in indirect food contact, that sanction will be maintained with the use of Ethanox 310 antioxidant. Its superior effectiveness and overall stability means that its use in most polymers greatly improves their capacity to process without degradation and to stand up to demanding long-term applications. Ethanox 330G antioxidant is a free-flowing, non-dusting, easy-to-use granular form of this very effective product. The product contains no binders.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³aerated
 0.745 g/cc0.0269 lb/in³packed
Molecular Weight 775.2 g/mol775.2 g/mol
Vapor Pressure <= 0.000667 bar
@Temperature 300 °C
<= 0.500 torr
@Temperature 572 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 244 °C471 °F
 
Descriptive Properties
AppearanceWhite crystalliner powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH496 / 315414

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.