MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi ABS 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: ABS is a strong filament ideal for 3D printing of solid printed products. Due to the process stability and physical features of Acrylonitrile Butadiene Styrene, it is a widely used thermoplastic polymer in industry. The material is also very light and durable. This makes ABS particularly suitable for tools, toys, and all kinds of utensils. Printed at a slightly over-average temperature for ABS, this filament gives extra strong 3D print results.

Material features:

  • Stable printing
  • Light and durable
  • Limited warping
Colors: ABS is available from stock in 26 bright colors. Other colors on request

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccISO 1183
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.0 MPa3770 psi3D-Printed Z
 36.0 MPa5220 psiInjection Molded
 36.0 MPa5220 psi3D-Printed X-Y
Tensile Strength, Yield 26.0 MPa3770 psi3D-Printed Z
 42.0 MPa6090 psi3D-Printed X-Y
 44.0 MPa6380 psiInjection Molded
Elongation at Break 2.0 %2.0 %3D-Printed Z
 6.0 %6.0 %3D-Printed X-Y
 8.0 %8.0 %Injection Molded
Elongation at Yield 2.0 %2.0 %3D-Printed Z
 3.0 %3.0 %Injection Molded
 3.0 %3.0 %3D-Printed X-Y
Modulus of Elasticity 1.80 GPa261 ksiYoung's, 3D-Printed Z
 1.90 GPa276 ksiYoung's, 3D-Printed X-Y
 2.30 GPa334 ksiYoung's, Injection Molded
Charpy Impact, Notched 2.20 J/cm²10.5 ft-lb/in²ISO 1791eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 235 - 255 °C455 - 491 °FISO 294
Vicat Softening Point 96.0 °C205 °FISO 306 B50
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 - 255 °C455 - 491 °FPrinting Temperature
 
Descriptive Properties
Bed Temp=90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9800 / 301025

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.