MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro Bayflex® 5110 Polyurethane Foam System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Bayflex 5110 is a water-blown polyurethane semi-flexible foam system.

Properties / Applications: Bayflex 5510 is a water-blown polyurethane semi-flexible foam system designed as back-fill support for vinyl extrusion, especially window lineals. This system is capable of filling 16-foot long extrusions, including cavities with small cross sections. As with any product, use of Bayflex 5110 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability for use.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity >= 1.02 g/cc>= 1.02 g/ccPoly 5110 Neutral (Component B)
 1.23 g/cc1.23 g/ccISO 6000 (Component A)
Viscosity 135 cP135 cPISO 6000 (Component A)
 1300 - 2000 cP1300 - 2000 cPPoly 5110 Neutral (Component B)
 
Processing PropertiesMetricEnglishComments
Gel Time 2.33 - 2.83 min2.33 - 2.83 min
 
Descriptive Properties
AppearanceDark brown liquidISO 6000 (Component A)
 Milky white liquidPoly 5110 Neutral (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Baynat® 3002 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-6718 Polyurethane Foam
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 20 pcf

PCOVEST0133 / 201916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.