MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BEC Materials C5 Resin LH100-1 Adhesives/Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: C5 is one of the main ingredients to compound with SIS for adhesive. It is obtained through cationic polymerization first and then hydrogenation process. C5 hydrogenation petroleum resin has lighter color, better performance in anti-aging, smell and compatibility. LH100-1 has lighter color than LH100-2.

Application: Adhesives/Coating

Formula:
C5(LH100-1): 15-25
SIS: 30-35
Terpene Resins: 30-35
Naphthenic Oil 4010: 10-15
Antioxidants: 1-2

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity <= 250 cP
@Temperature 190 °C
Ash <= 0.0020 %
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.50[KOH mg/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 95.0 - 105 °C
Flash Point >= 210 °C
 
Optical PropertiesOriginal ValueComments
Yellow Index 3.5 - 9.49 %
 
Descriptive Properties
Antioxygen=0.3%
Bromine Value=3.0 Br2g/100g
Fire Point=220°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBECM001 / 306954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.