MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adsyl 7572 XCP Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade (Polyolefin)

Material Notes: Adsyl resins are propylene plus ethylene and butene based random copolymers and terpolymers with high comonomer ratios that deliver improved sealing properties. Grades of Adsyl resins can be used in all of the main film extrusion technologies, such as BOPP, Double Bubble, Cast and Blown Film. Adsyl grades are mainly used for skin layers in co-extruded or coated film structures to provide sealing functionality.

Adsyl 7572 XCP is an advanced polyolefin, specially designed for use as a sealing layer in coextruded film applications.

This grade features a very low seal initiation temperature (<100°C) and excellent optical properties. It does not contain slip or anti-block additives. Applications: Barrier Film, Clarity Film, Food Packaging Film, Lamination Film, Sealants, Shrink Film, Specialty Film, Stationery Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccMethod A; ISO 1183
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 14.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-1,-3
Film Tensile Strength at Yield, TD 14.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-1,-3
Film Elongation at Break, MD 850 %
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Break, TD 900 %
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Yield, MD 16 %
@Thickness 0.0500 mm
500 mm/min, cast film; ISO 527-3
Film Elongation at Yield, TD 14 %
@Thickness 0.0500 mm
500 mm/min, cast film; ISO 527-3
Secant Modulus, MD 0.260 GPa
@Thickness 0.0500 mm
23 mm/min, cast film; ISO 527-1,-3
Secant Modulus, TD 0.250 GPa
@Thickness 0.0500 mm
23 mm/min, cast film; ISO 527-1,-3
Film Tensile Strength at Break, MD 37.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Tensile Strength at Break, TD 41.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Heat Seal Strength Initiation Temperature 92.0 °CLYB method
 
Thermal PropertiesOriginal ValueComments
Melting Point 128 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 103 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 0.20 %
@Thickness 0.0500 mm
ASTM D 1003
Gloss 92 %
@Thickness 0.0500 mm
45°; ASTM D 2457
 
Descriptive Properties
Processing MethodBOPP, Cast Film, Double Bubble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adsyl 5 C 30 F ST Polyolefin
LyondellBasell Adsyl 6 C 30 F Polypropylene terpolymer
LyondellBasell Adsyl™ 5 C 30 F Polyolefin
LyondellBasell Adsyl™ 3 C 30 F HP Polypropylene Copolymer
LyondellBasell Adsyl 7641 XCP Polypropylene terpolymer

PEQT7044 / 218683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.