MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SK Chemicals SKYGREEN® JN400 PETG Copolymer Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: SKYGREEN J has exceptional chemical resistance. Suited to a variety of applications including home appliances, SKYGREEN J maintains long-lasting clarity even under the toughest conditions. SKYGREEN PETG is transparent, chemically resistant, and easily processable.

Property data for injection molded samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength at Break 53.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 45.0 MPa50 mm/min; ASTM D638
Elongation at Break 340 %50mm/min; ASTM D638
Elongation at Yield 5.0 %50 mm/min; ASTM D638
Flexural Strength 67.0 MPa1.27 mm/min; ASTM D790
Flexural Modulus 1.80 GPa1.27 mm/min; ASTM D790
Izod Impact, Notched NBASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Transmission, Visible 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSK000f / 243201

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.