MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® FE270038 BK267 PA66-(GF+MD)40  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Mineral Filled

Material Notes: 40% Glass/Mineral Reinforced Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccDAM; ISO 1183
Melt Density 1.30 g/cc
@Temperature >=245 °C
Water Absorption 5.0 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.50 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa50% RH; ISO 527-1/-2
 145 MPaDAM; ISO 527-1/-2
Elongation at Break 2.5 %DAM; ISO 527-1/-2
 2.6 %50% RH; ISO 527-1/-2
Tensile Modulus 7800 MPa50% RH; ISO 527-1/-2
 8800 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.34DAM; ISO 527-1/-2
 0.3450%RH; ISO 527-1/-2
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 41.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 41.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
Tensile Creep Modulus, 1 hour 7000 MPa50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 6000 MPa50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cm50% RH; IEC 62631-3-1
 1.00e+14 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 3.00e+14 ohm50% RH; IEC 62631-3-2
Dielectric Strength 41.0 kV/mm50% RH; IEC 60243-1
 41.0 kV/mmDAM; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.28 J/g-°C
@Temperature >=245 °C
Melt
Thermal Conductivity 0.260 W/m-K
@Temperature >=245 °C
Melt
Melting Point 245 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 230 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °CInjection Optimum
 280 - 300 °CInjection
Mold Temperature 70.0 - 120 °CInjection
 100 °CInjection Optimum
Ejection Temperature 210 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 4.00 hourDehumidified Dryer
Moisture Content 0.20 %
Hold Pressure 50.0 - 100 MPa
 
Descriptive Properties
Delivery formPellets
Drying Recommendedyes
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3
Max. screw tangential speed (m/s)0.2DAM
Part Marking CodePA66-(GF+MD)40ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66-(GF+MD)40ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Minlon® EFE6053 BK413 PA66-(GF+MD)40
BASF Nypel® RC6024 BK 30% Mineral/Glass Filled PA6 (Dry)
DuPont Mobility and Materials Zytel® FE270050 BK099 PA66-(GF+MD)30
Akro-Plastic Akromid® B3 LA black (4056) PA6, DAM
Celanese Zytel® FR50 NC010 PA66-GF25FR(17)

PDSX5394 / 198034

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.