Pyro Log is the only 152mm thick, high purity, needled blanket available in standard uncompressed densities up to 240kg/m3. Vertically-fiberized Pyro-Log fiber is of exceptional uniformity of dimensions and of naturally low shot content. Pyro-Log offers a unique solution to the problems encountered in designing linings for use in the toughest of furnace environments. Applications: Pyro Log has a multitude of uses in heat containment applications in all industry groups, a selection of which are as follows: - Ceramic Industry (kiln car insulation - furnace floors)
- Iron and Steel (walking beam furnace skid rail insulation)
- General (engineered shapes)
- Pyro-Log is the precursor material for the Pyro-Bloc range of mechanically fixed modules
Information provided by Morgan Advanced Materials |