MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sumitomo Bakelite SUMILITERESIN® PR-51587 I Phenolic resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: SUMILITERESIN® PR-51587 I is a tall oil modified phenolic resin with flake shape. It contains modified tall oil to improve flexibility properties. It is generally applied for tire and rubber as reinforcement.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 62.0 - 72.0 °C144 - 162 °FMettler
Softening Point 85.0 - 92.0 °C185 - 198 °FB&R
 
Processing PropertiesMetricEnglishComments
Gel Time 0.330 - 0.750 min
@Temperature 165 °C
0.330 - 0.750 min
@Temperature 329 °F
resin/hexamine = 100/8
 
Descriptive Properties
AppearanceBrown - Flake
Flow Distance50-90mm, 125°C; resin/hexamine = 100/8
Free Phenol, GC, %< 3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT603 / 194408

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.