MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTAPEEK® XDT PEEK/X-Ray Detectable
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:
  • X-ray detectable as small as 3 mm particle size
  • Excellent impact and wear resistance
  • High Temperature Applications
Product applications:
  • Food processing parts
  • Bakery machinery
  • Tortilla processing

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D2240
Tensile Strength, Yield 100 MPa14500 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM D696
Melting Point 332 °C630 °FASTM D789
Maximum Service Temperature, Air 249 °C480 °F
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF YesYes
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9058 / 232761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.