MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lanxess THERBAN® AT 3443 VP Butadiene Acrylonitrile Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A low viscosity, partially hydrogenated butadiene acrylonitrile copolymer designed primarily for dynamic applications requiring excellent requiring excellent resistance to heat, ozone and non polar hydrocarbon fluids. Sulfur curing systems are used for improved dynamic properties and adhesion to steel and textile reinforcing materials. However, peroxide/coagent systems can be used for improved resistance to heat and compression set. Low viscosity AT-technology provides a broad processing window, low mold fouling and the potential for higher filler loads compared to standard viscosity HNBR types.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³
Volatiles <= 0.70 %<= 0.70 %ASTM D5668
Mooney Viscosity 34 - 44
@Temperature 100 °C
34 - 44
@Temperature 212 °F
(1+4); ASTM D1646
Ash <= 0.49 %<= 0.49 %ASTM D5667
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month
@Temperature <=35.0 °C
36.0 Month
@Temperature <=95.0 °F
 
Descriptive Properties
ColorLight brown
Content32.5-35.5%Acrylonitrile, ISO 24698-1
 3-5%Residual double bonds

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATG s.r.l. HNBR Hydrogenated Nitrile Butadiene Rubber
Lanxess THERBAN® 3668 VP Butadiene Acrylonitrile Copolymer
Lanxess THERBAN® 3607 Butadiene Acrylonitrile Copolymer
Hydrogenated Nitrile Rubber (HNBR)
Evonik Vestamid®/Trogamid® RD 5080 HNBR Rubber/Plastic Composite

PLANY9079 / 209470

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.